In MIG welding, selecting the right welding wire is only one part of achieving consistent weld quality. Even when using a suitable consumable such as 70S-6 welding wire, incorrect machine settings, poor surface preparation, improper shielding gas coverage and inconsistent welding techniques can lead to defects.
For fabricators, production engineers and industrial manufacturers, these mistakes can result in rework, material wastage, additional grinding, production delays and compromised weld integrity.
70S-6 welding wire is commonly used for carbon and mild steel fabrication. Its manganese and silicon content provides deoxidizing capability that can help manage certain surface conditions. However, it cannot compensate for every welding problem.
Understanding common MIG welding mistakes and correcting their underlying causes helps improve welding consistency, productivity and finished weld quality.
1. Welding on Unprepared or Contaminated Metal Surfaces
One of the most common MIG welding mistakes is starting the welding process without properly preparing the base material.
Steel surfaces may contain rust, mill scale, oil, grease, paint, moisture or other contaminants. These substances can interfere with the welding arc and molten weld pool, increasing the possibility of porosity, spatter and inconsistent weld appearance.
ER70S-6 welding wire contains relatively higher levels of manganese and silicon deoxidizers than some other solid carbon-steel wire classifications. These elements help manage certain oxidizing conditions during welding.
However, this does not mean that the wire should be used as a replacement for proper cleaning.
How to avoid this mistake:
- Remove oil, grease, paint and moisture before welding.
- Clean excessive rust and mill scale wherever required by the welding procedure.
- Use suitable grinding or wire-brushing methods.
- Inspect the joint area before starting production welding.
- Maintain consistent surface preparation across production batches.
Practical takeaway: The deoxidizing properties of 70S-6 wire provide useful process tolerance, but clean base metal remains essential for dependable weld quality.
2. Using Incorrect Voltage and Wire Feed Speed
Voltage and wire feed speed (WFS) are two important parameters in MIG welding.
Wire feed speed controls the rate at which the electrode enters the welding arc and strongly influences welding current. Voltage affects arc length and the characteristics of the molten weld pool.
An incorrect combination can produce an unstable arc, excessive spatter, poor penetration or an irregular weld bead.
For example:
- Excessive wire feed speed relative to voltage can cause wire stubbing and an unstable arc.
- Insufficient wire feed speed for the selected voltage can create an excessively long arc and an inconsistent bead.
- Incorrect voltage settings can produce an overly convex or excessively flat weld profile.
How to avoid this mistake:
- Start with the welding parameters recommended for the selected wire diameter and shielding gas.
- Check the welding machine manufacturer’s parameter chart.
- Adjust voltage and wire feed speed together rather than independently guessing.
- Perform trial welds on representative material thicknesses.
- Record approved settings for repeat production jobs.
There is no single voltage or wire feed speed suitable for every 70S-6 welding application. Parameters must be established according to wire diameter, material thickness, joint design, transfer mode and welding position.
3. Ignoring Shielding Gas Selection and Coverage
Shielding gas protects the molten weld pool from atmospheric contamination. Incorrect gas selection or inadequate gas coverage can lead to porosity, unstable arc behaviour and excessive spatter.
Solid ER70S-6 wires are commonly used with carbon dioxide (CO₂) or argon-CO₂ shielding gas mixtures, subject to the manufacturer’s recommendations.
Common mistakes include:
- Using an unsuitable shielding gas for the selected welding procedure.
- Setting incorrect gas flow.
- Welding in areas exposed to strong air drafts.
- Ignoring leaks in gas hoses and connections.
- Allowing excessive spatter to accumulate inside the gas nozzle.
How to avoid this mistake:
- Confirm gas compatibility with the wire manufacturer’s technical documentation.
- Check the regulator, flowmeter and hose connections.
- Keep the welding nozzle clean.
- Protect the welding area from drafts.
- Verify that shielding gas reaches the weld pool consistently.
Increasing gas flow is not always the solution. Excessive flow can create turbulence and draw surrounding air into the shielding zone. Use the appropriate flow range for the nozzle, setup and working conditions.
4. Maintaining Incorrect Gun Angle and Stickout
Welding gun position affects arc direction, shielding coverage, penetration and bead formation.
Two important factors are gun angle and contact-tip-to-work distance (CTWD), also commonly discussed in relation to electrode extension or stickout.
An excessively steep gun angle can disturb shielding gas coverage and change how the arc interacts with the weld pool. Excessive stickout can increase electrical resistance in the electrode extension and affect welding current and arc stability.
How to avoid this mistake:
- Maintain a consistent gun angle appropriate for the joint and welding position.
- Follow the recommended CTWD for the selected wire and transfer mode.
- Avoid unnecessarily extending the wire beyond the contact tip.
- Keep the gun movement controlled throughout the weld.
- Follow the welding procedure specification (WPS), where applicable.
A consistent gun position helps maintain more predictable welding conditions, especially during repetitive fabrication work.
5. Welding Too Fast or Too Slowly
Travel speed determines how quickly the welding arc moves along the joint. It directly affects heat input per unit length, weld bead dimensions and the amount of deposited metal.
Moving too quickly can produce a narrow bead, insufficient fusion or an uneven weld profile. Moving too slowly can create excessive weld buildup, increased heat input and potential burn-through on thinner materials.
How to avoid this mistake:
- Maintain a consistent travel speed.
- Keep the arc directed towards the leading edge of the weld pool.
- Observe the weld pool instead of focusing only on the wire.
- Avoid unnecessary weaving.
- Adjust travel speed according to material thickness, joint geometry and approved welding parameters.
For production welding, consistent travel speed is particularly important because variations can create inconsistent weld dimensions across multiple components.
6. Choosing the Wrong Wire Diameter for the Application
Selecting a welding wire based only on availability or price can create unnecessary welding difficulties.
Wire diameter influences the current range, deposition rate, feeding behaviour and suitability for different material thicknesses.
A wire diameter that is unsuitable for the application may make it difficult to control the weld pool, particularly when welding thin sheets or thicker structural components.
Before selecting 70S-6 welding wire, consider:
- Base-metal grade and thickness.
- Joint configuration and welding position.
- Welding machine output capacity.
- Required deposition rate.
- Welding procedure requirements.
- Wire diameter and shielding gas compatibility.
For industrial procurement teams, it is equally important to confirm the actual product classification, dimensional tolerance, chemical composition and applicable inspection documentation with the manufacturer.
7. Neglecting Welding Equipment and Wire Feeding Maintenance
A good welding wire cannot deliver consistent results if the feeding system is not maintained properly.
Worn contact tips, incorrect drive-roll pressure, damaged liners, clogged nozzles and poor spool installation can interrupt wire feeding.
These problems may result in:
- Irregular wire feed.
- Arc instability.
- Excessive spatter.
- Burnback.
- Inconsistent weld bead formation.
How to avoid this mistake:
- Inspect contact tips regularly.
- Clean the welding gun nozzle.
- Check drive-roll alignment and pressure.
- Replace damaged or worn liners.
- Ensure the wire spool is installed correctly.
- Inspect the feeding system whenever unexpected arc instability occurs.
Preventive equipment maintenance helps reduce avoidable interruptions during repetitive welding operations.
8. Ignoring Welding Wire Storage and Handling
Welding wire quality can be affected by unsuitable storage and handling conditions.
Dust, moisture, oil and other contaminants may accumulate on exposed wire surfaces. These contaminants can interfere with feeding and welding performance.
Incorrect handling can also damage the spool or affect wire unwinding.
How to avoid this mistake:
- Store welding wire in its original packaging until required.
- Keep opened spools in a clean, dry environment.
- Avoid contact with oil, grease and moisture.
- Follow the manufacturer’s storage and handling instructions.
- Inspect wire condition before loading it into the welding machine.
For manufacturers operating multiple welding stations, standardised consumable storage practices can help improve consistency between production shifts.
Common MIG Welding Defects and Their Possible Causes
Understanding the relationship between welding mistakes and visible defects helps operators troubleshoot problems more effectively.
| MIG welding defect | Possible causes | Corrective action |
| Porosity | Poor shielding, contaminated surfaces, gas leaks | Clean the joint and inspect gas coverage |
| Excessive spatter | Incorrect voltage/WFS, poor gas coverage, excessive stickout | Check parameters, gas supply and gun setup |
| Lack of fusion | Insufficient heat, incorrect travel speed or gun angle | Review parameters and joint technique |
| Burn-through | Excessive heat input or slow travel speed | Adjust heat input and travel speed |
| Convex weld bead | Incorrect parameters or unsuitable travel conditions | Review voltage, WFS and travel speed |
| Irregular bead | Inconsistent movement or unstable wire feeding | Inspect technique and feeding equipment |
These are possible causes rather than universal diagnoses. Multiple variables can produce similar defects, so corrections should be based on inspection and controlled parameter adjustments.
Why Correct 70S-6 Welding Wire Selection Matters
70S-6 welding wire is commonly considered for mild and carbon steel fabrication because of its deoxidizing characteristics and suitability for a range of gas metal arc welding applications.
However, selecting the correct consumable requires more than matching the wire designation.
Industrial buyers and fabrication companies should evaluate:
- Classification against the applicable AWS specification.
- Base-metal compatibility.
- Chemical composition and mechanical property requirements.
- Available wire diameters.
- Shielding gas recommendations.
- Wire feeding consistency.
- Manufacturer test certificates and inspection documentation.
- Suitability for the intended welding procedure.
The American Welding Society’s AWS A5.18/A5.18M specification establishes classification requirements for carbon steel electrodes and rods used in gas-shielded arc welding. Buyers should refer to the applicable edition and verify product documentation before approving a consumable for critical applications.
Choosing the Right Welding Wire for Consistent Production
For industrial manufacturers, welding quality depends on the combined performance of the consumable, equipment, operator and approved welding procedure.
At STRONGWIRE, the STRONG 70 SERIES product range includes STRONG 70S6, which the company identifies for welding mildly contaminated or rusty steel surfaces.
When evaluating welding consumables for fabrication or manufacturing requirements, buyers should consider product classification, application compatibility, technical documentation and quality requirements rather than relying on the designation alone.
Explore the STRONG 70 SERIES welding wires to understand the available product range.
Conclusion
Avoiding common MIG welding mistakes requires a systematic approach to consumable selection, machine settings, surface preparation, shielding gas management and equipment maintenance.
Even when using 70S-6 welding wire, poor welding practices can result in porosity, excessive spatter, lack of fusion and inconsistent weld bead formation.
For fabricators and industrial manufacturers, the best approach is to establish suitable welding parameters, follow approved procedures, maintain equipment and inspect consumables regularly.
Selecting an appropriate welding wire from a reliable manufacturer is another important step towards maintaining consistent production quality.